铜冶炼烟尘碱浸除砷试验研究Removal of Arsenic in Copper Smelting Dust by Alkaline Leaching
吴星琳;罗仁昆;李涛;陈杭;葛素志;衷水平;王俊娥;
摘要(Abstract):
研究了碱性体系中铜冶炼烟尘的选择性脱砷。根据热力学计算结果推测,砷可溶于碱性体系,且过量的碱会导致铜、铅复溶。试验结果表明:在碱初始质量浓度100 g/L、温度80℃、液固体积质量比5∶1、反应时间2 h条件下,烟尘经二级逆流浸出,砷浸出率达94%以上,开路浸出液中铜、铅质量浓度分别降至0.03和0.05 g/L左右,实现了选择性高效脱砷。
关键词(KeyWords): 铜冶炼烟尘;砷;热力学;选择性;去除
基金项目(Foundation): 固体废弃物资源化利用福建省高校工程研究中心开放基金资助项目(LYGF-2017)
作者(Authors): 吴星琳;罗仁昆;李涛;陈杭;葛素志;衷水平;王俊娥;
DOI: 10.13355/j.cnki.sfyj.2019.06.013
参考文献(References):
- [1] 张秋芳,施贤蛟.铜烟灰处理方案探讨[J].有色矿冶,1999(5):54-57.
- [2] YAN W.Study on leaching of dust of copper flash smelting furnace[J].Metallurgical Engineering,2015,2(3):151-157.
- [3] 李利丽.铜冶炼高砷烟灰综合处理流程研究[J].中国金属通报,2011(19):42-43.
- [4] 张荣良,丘克强,谢永金等.铜冶炼闪速炉烟尘氧化浸出与中和脱砷[J].中南大学学报(自然科学版),2006,37(1):73-78.
- [5] 孙乐栋,李杰,光明等.炼铜烟灰硫酸浸出及铜浸出动力学研究[J].矿冶工程,2016,36(1):97-100.
- [6] GUO X Y,YI Y,SHI J,et al.Leaching behavior of metals from high-arsenic dust by NaOH-Na2S alkaline leaching[J].Transactions of Nonferrous Metals Society of China,2016,26(2):575-580.
- [7] 李思唯,刘志宏,刘智勇,等.铜闪速熔炼电收高砷烟尘硫酸化焙烧脱砷试验研究[J].湿法冶金,2017,36(4):336-341.
- [8] 刘海浪,和森,宋向荣,等.铜冶炼高砷烟尘浸出特性研究[J].安全与环境学报,2017,17(3):1124-1128.
- [9] KARIMOV K A,NABOICHENKO S S.Sulfuric acid leaching of high-arsenic dust from copper smelting[J].Metallurgist,2016,60(3):456-459.
- [10] XU Z F,LI Q,NIE H P.Pressure leaching technique of smelter dust with high-copper and high-arsenic[J].Transactions of Nonferrous Metals Society of China,2010,20(1):176-181.
- [11] 杨贵生.用碳酸钠溶液从铜冶炼烟尘中脱除砷试验研究[J].湿法冶金,2019,38(3):235-238.
- [12] 王绍宇,秦庆伟,刘文科,等.用氢氧化钠溶液从澳斯麦特熔炼烟尘中选择性浸出砷锑铅锌[J].湿法冶金,2018,37(3):198-201.
- [13] 易宇,石靖,田庆华,等.高砷烟尘氢氧化钠-硫化钠碱性浸出脱砷[J].中国有色金属学报,2015,25(3):806-814.
- [14] 李洪桂.湿法冶金学[M].长沙:中南大学出版社,2005:38-122.
- [15] ANDERKO A,SANDERS S J,YOUNG R D.Real-solution stability diagrams:a thermodynamic tool for modeling corrosion in wide temperature and concentration ranges[J].Corrosion Science,1997,53(1):43-53.
- [16] KINNIBURGH D G,COOPER D M.Predominance and mineral stability diagrams revisited[J].Environmental Science & Technology,2004,38(13):3641-3648.
- [17] YOU H X,XU H B,ZHANG Y,et al.Potential-pH diagrams of Cr-H2O system at elevated temperatures[J].Transactions of Nonferrous Metals Society of China,2010,20(S1):26-31.
- [18] FISHTIK I.Thermodynamic stability relations in redox systems[J].Environmental Science & Technology,2006,40(6):1902-1910.
- [19] MU W Z,ZHANG T A,LIU Y,et al.E-pH diagram of ZnS-H2O system during high pressure leaching of zinc sulfide[J].Transactions of Nonferrous Metals Society of China,2010,20(10):2012-2019.
- [20] JIN Z N,JIANG K X,WEI X J,et al.Potential-pH diagrams of As-S-H2O system at high temperature[J].Mining and Metallurgy,1999,4(8):46-50.
- [21] HE Y L,XU R D,HE S W,et al.φ-pH diagram of As-N-Na-H2O system for arsenic removal during alkaline pressure oxidation leaching of lead anode slime[J].Transactions of Nonferrous Metals Society of China,2017,27(3):676-685.
- [22] 朱元保,沈子深,张传福,等.电化学数据手册[M].长沙:湖南科学技术出版社,1985:135-164.